Grade UNS Indian / IS European / EN %C %Mn %P %S %Si %Cr %Ni %Mo % Others
(Max) (Max) (Max) (Max) (Max)
SS410 S41000 X12Cr12 1.4006 0.08-0.15 1.00 0.040 0.030 1 11.50-13.50 0.75 max
SS415 S41500 X02Cr13Ni4Mn1Mo1 1.4313 0.05 0.50-1.00 0.030 0.030 0.6 11.50-14.00 3.50-5.50 0.50-1.00
SS420 S42000 X20Cr13 1.4021 0.15 min 1.00 0.040 0.030 1 12.00-14.00 0.75 max 0.50 max
SS420J1 X20Cr13 1.4021 0.16-0.25 1.00 0.040 0.030 1 12.00-14.00 0.6
SS420J2 X30Cr13 1.4028 0.26-0.40 1.00 0.040 0.030 1 12.00-14.00 0.6
SS420MoV 1.4116 0.45-0.55 1.00 0.040 0.015 1 14.00-15.00 0.50-0.80 V=0.10-0.20
SS431 S43100 X15Cr16Ni2 1.4057 0.2 1.00 0.040 0.030 1 15.00-17.00 1.25-2.50
BS 0.6-0.7 1.00 0.028 0.020 0.75 12.50-13.50
SS405 S40500 X04Cr12Al 1.4002 0.08 1.00 0.040 0.030 1 11.50-14.50 0.6 AI=0.10-0.30